Size Range
Outside Diameter (OD) | Wall Thickness |
.250”–1.000” | .035″–.065″ |
Cold finished and bright annealed tube.
Chemical Requirements
Alloy 904L (UNS N08904) Composition %
C Carbon | Mn Manganese | P Phosphorus | S Sulfur | Si Silicon | Cr Chromium | Ni Nickel | Mo Molybdenum | N Nitrogen | Cu Copper |
0.020 max | 2.00 max | 0.040 max | 0.030 max | 1.00 max | 19.0–23.0 | 23.0–28.0 | 4.0–5.0 | 0.10 max | 1.00–2.00 |
Dimensional Tolerances
OD | OD Tolerance | Wall Tolerance |
≤ .500″ | ± .005” | ± 15% |
0.500”–1.500” | ± .005” | ± 10% |
Mechanical Properties
Yield Strength: | 31 ksi min |
Tensile Strength: | 71 ksi min |
Elongation (min 2"): | 35% |
Hardness (Rockwell B Scale): | 90 HRB max |
Fabrication
Alloy 904L is non-magnetic in all conditions and has excellent formability and weldability. The austenitic structure also gives this grade excellent toughness, even down to cryogenic temperatures.
Industry Applications
Chemical Process
Its high chromium and nickel content, along with the addition of molybdenum and copper, help alloy 904L stand up to sulfuric, phosphoric and acetic acids. This is especially useful in the production of acids and fertilizers.